Anzahl der Publikationen: 10
2021
Yuan, Jieyan; Zhou, Xin; Dong, Shujuan; Jiang, Jianing; Deng, Longhui; Song, Wenjia; Dingwell, Donald B. und Cao, Xueqiang
(2021):
Tailoring the initial characterization of fully stabilized HfO2 with Y2O3/Ta2O5.
In: Journal of Alloys and Compounds, Bd. 867, 159113
Yuan, Jieyan; Zhou, Xin; Dong, Shujuan; Jiang, Jianing; Deng, Longhui; Song, Wenjia; Dingwell, Donald B. und Cao, Xueqiang
(2021):
Plasma sprayed 18mol% YO1.5 stabilized hafnia as potential thermal barrier coating.
In: Ceramics International, Bd. 47, Nr. 10: S. 14515-14526
2020
Zhang, Hao; Yuan, Jieyan; Song, Wenjia; Zhou, Xin; Dong, Shujuan; Duo, Shuwang; Wang, Jinshuang; Yang, Xiong; Jiang, Jianing; Deng, Longhui; Huang, Jingqi und Cao, Xueqiang
(2020):
Composition, mechanical properties and thermal cycling performance of YSZ toughened La2Ce2O7 composite thermal barrier coatings.
In: Ceramics International, Bd. 46, Nr. 5: S. 6641-6651
Zhang, Hao; Zeng, Jinyan; Yuan, Jieyan; Liang, Panpan; Zhou, Xin; Chen, Si; Duo, Shuwang; Dong, Shujuan; Jiang, Jianing; Deng, Longhui und Cao, Xueqiang
(2020):
Spray power-governed microstructure and composition, and their effects on properties of lanthanum-cerium-tantalum-oxide thermal barrier coating.
In: Ceramics International, Bd. 46, Nr. 11: S. 18114-18122
Cao, Xueqiang; Dong, Shujuan; Vassen, Robert; Wang, Jinshuang; Zou, Binglin; Li, Shibao; Hui, Yu; Yuan, Jieyan; Song, Wenjia; Cao, Qin; Jiang, Jianing; Deng, Longhui und Dong, Shujuan
(2020):
Degradation of zirconia in moisture.
In: Corrosion Science, Bd. 176, 109038
2019
Liu, Fan; Song, Wenjia; Zhou, Xin; Huo, Panjie; Yuan, Jieyan; Jiang, Jianing; Deng, Longhui; Dong, Shujuan und Cao, Xueqiang
(2019):
Microstructures, thermophysical properties and thermal cycling behavior of LaZnAl11O19 thermal barrier coatings deposited by atmospheric plasma spraying.
In: Inorganic Chemistry Frontiers, Bd. 6, Nr. 11: S. 3302-3314
Chen, Si; Song, Wenjia; Zhou, Xin; Zhang, Hao; Zhou, Xiong; Tu, Yunwei; Yuan, Jieyan; Dong, Shujuan und Cao, Xueqiang
(2019):
Hot corrosion of Mg2SiO4 ceramics exposed to V2O5 at temperatures of 700-1050 degrees C in air.
In: Corrosion Science, Bd. 159, UNSP 108114
Diese Liste wurde am